Wholesale PriceList for CV-709 silicone sealant for PV moudels to Armenia Importers
Short Description:
Description CV709 is a high-performance silicone sealant, one-component oxime type room temperature curing silicone rubber, has excellent weather resistance, high thixotropy, after curing for solar components involved in the base material has good caking property, by TUV for environmental requirements of the ROHS, UL E339949 Key Features 1. 100% silicone 2. No sag 3. high thixotropy 4. Water & weatherproof 5. For solar components involved in the base material has good bonding Basic Ap...
We will make every effort to be outstanding and perfect, and accelerate our steps for standing in the rank of international top-grade and high-tech enterprises for Wholesale PriceList for CV-709 silicone sealant for PV moudels to Armenia Importers, We welcome new and old customers from all walks of life to contact us for future business relationships and mutual success!
Description
CV709 is a high-performance silicone sealant, one-component oxime type room temperature curing silicone rubber, has excellent weather resistance, high thixotropy, after curing for solar components involved in the base material has good caking property, by TUV for environmental requirements of the ROHS, UL E339949
Key Features
1. 100% silicone
2. No sag
3. high thixotropy
4. Water & weatherproof
5. For solar components involved in the base material has good bonding
Basic Application
1.Solar module frame seal
2.The adhesive of the solar energy back to the terminal block
3.General industrial assembly with seal
Technical data sheet
Test standard | Test project | Unit | value |
Before curing——25℃,50%R.H. | |||
specific gravity | g/ml | 1.34-1.40 | |
GB13477 | Operating time | min | 15 |
GB13477 | surface drying time(25℃,50%R.H.) | min | 40-60 |
3 days after curing——25℃,50%R.H. | |||
Temperature range | ℃ | -55~200 | |
GB13477 | Durometer Hardness | Shore A | 40~55 |
The ultimate tensile strength | Mpa | ≥2 | |
GB13477 | Breaking elongation | % | 300-600 |
Aluminum bonding shear strength | Mpa | ≥1.5 | |
Electrical properties | |||
Breakdown voltage | Kv/mm | ≥20 | |
Volume resistance | ohm.cm | 9E+14 | |
Dielectric constant | 3.1@50Hz |
Certification
UL E339949; TUV
Color
Black, White
Package
300ml in cartridge * 24 per box, 500ml in sausage *20 per box
Shelf life
12 months
Note
If you want the TDS or MSDS or other details, please contact with our sales person.
Be sure to subscribe to my sponsor Cottage Life! Check out their channel here: https://www.youtube.com/user/CottageLifeMagazine
Here’s their Floating Hot Tub video, pretty sweet: https://youtu.be/zApeT-AebMg
v v v v v v v Click ‘Show more’ v v v v v v v
I took up running these past few years as an extra hobby to allow me some thinking time away from the computer and all my camera gear. I looked into purchasing some of these minimalist shoes both for running as well as for a water shoe for fishing but found that my local stores didn’t carry any in stock, and buying shoes online can be risky for fitting purposes. Why not make some myself then?
I didn’t believe that spray rubber would work very well at first and assumed that I would have to use the liquid paint-on variety that comes in a tin to achieve a good coating on the fabric, but after testing the spray rubber for myself I didn’t even bother with any other method. It works excellent. The rubber is more durable than expected, and after about a quarter mile on very sharp gravel I noticed no wear at all.
One issue that I do have with the shoes is that some of the rubber solvent absorbed into the fabric outside the spray area, carrying trace amounts of rubber with it. This was due to my impatience in adding too much rubber in the first coat which wet the fabric too much and caused unsightly stains that you can see on top of the toes in the video, and also caused a little bit of extra stiffness in those areas. This should be an avoidable issue by simply going a little more slowly until there is a good rubber surface established over the absorbent fabric. There shouldn’t be much to worry about after the first coat or two is added.
One other very minor improvement I would make in my next pair of shoes is to make the heel more narrow while spraying on the rubber. While I shaped the socks fairly accurately to the natural shape of my feet, I would have preferred the heel to be a little narrower so that it was a snugger fit. That’s mostly a matter of preference and doesn’t contribute one way or the other toward function.
Items used for this project:
Divided Toe Socks
Spray Rubber
Plastic Grocery Bags
Coat Rack (Or anything else that can hold the socks upright – two sticks would do fine)
Fan (For both ventilation as well as increasing solvent drying time) #NightHawkInLight
-~-~~-~~~-~~-~-
Check out my latest video: “How To View Invisible Air Currents With Lasers”
-~-~~-~~~-~~-~-