Wholesale Discount Siway MG PU FOAM to Turkey Manufacturers
Short Description:
Description MG PU FOAM is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength; Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins; Key Features 1. Noise silencing effect 2. Strong bonding strength 3. Water & weatherproof 4. Primerless adhesion to most building materials Basic Application 1.Doors and Windows and...
With our rich experience and considerate services, we have been recognized as a reliable supplier for many international buyers for Wholesale Discount Siway MG PU FOAM to Turkey Manufacturers, We look forward to establish a long-term business relationship with your esteem co-operation.
Description
MG PU FOAM is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength;
Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins;
Key Features
1. Noise silencing effect
2. Strong bonding strength
3. Water & weatherproof
4. Primerless adhesion to most building materials
Basic Application
1.Doors and Windows and wall body between the gap filling sealing, fixed bond
2.Language lab, studio, etc when decorating, gap to fill
Technical data sheet
Project |
Value |
||
Density, Kg/m³,Not less |
10 |
||
Thermal conductivity,35℃,W/(m·K) no more than |
0.050 |
||
Dimensional stability(23±2)℃,48,h no more than |
5 |
||
Operating temperature |
-10~+35℃ |
||
Optimum operating temperature |
+18~+25℃ |
||
Temperature range(After curing) |
-35~+80℃ |
||
Tensile bond strength kPa Not less |
Aluminum plate |
Standard condition,7d |
80 |
Immersion,7d |
60 |
||
PVC plate |
Standard condition,7d |
80 |
|
Immersion,7d |
60 |
||
Cement Plate |
Standard condition,7d |
60 |
|
Shear strength,kpa,Not less |
80 |
||
Foam expansion ratio,Not less |
Standard value-10 |
Certification
JC 936-2004
Color
White
Package
750ml in Bottle * 12 per box
Shelf life
12 months
Note
If you want the TDS or MSDS or other details, please contact with our sales person.
Even though it is possible for your commercial inflatable bounce house to become damaged, there is no need to worry! Watch this super quick and easy video to learn how to properly patch and repair your damaged inflatable using a vinyl cement repair kit, without having to ship it out and pay for the repair.
☞ Website: https://MagicJump.com
Follow, Like, Share & More:
ツ Subscribe!: https://www.youtube.com/subscription_center?add_user=MagicJumpInc
ツ Twitter: https://twitter.com/MagicJump
ツ Facebook: https://facebook.com/MagicJump
ツ Blog: https://magicjump.wordpress.com/
____________________________________________
Disclaimer: All views, opinions, or advice presented in this video are those of Magic Jump, Inc. The purpose of this video is solely to inform the viewer of all Magic Jump, Inc. knows thus far about this specific topic from years of personal experience. Due to the nature of this website, this video is current only at the time it was initially posted and may contain information that can be outdated. The viewer is responsible for doing all further research about the accuracy, reliability, completeness, suitability, and availability of the information you receive from this video. You, the viewer, are to use the information given at your own free will, and at your own risk. This video does not offer any sort of legal or professional advice. Exercise extreme caution and good judgment when performing any of the actions shown in this video. Magic Jump, Inc. is not liable for any injuries or damages incurred while attempting to follow any suggestions given in this video.
The top 10 things you need to know about what NOT to do with your glue gun, brought to you by the Slurpee my husband brought me back from 7-11. (This is not a sponsored post, just an explanation.)
As Promised, Here’s the list as text in case you can’t keep up
10. Never pull a glue stick you have inserted out of the back of the glue gun, since you might pull hot glue out and hurt yourself. Also, you could break the feeder mech, and thus, your glue gun.
9. Never lay the glue gun on it’s side. The glue could leak out the back of the heating element and burn you when you pick it back up again.
8. Don’t leave your glue gun plugged in while unattended.
7. Do not use your glue gun on an uneven surface since it could fall over/off.
6. Do not leave cords dangling where children or animals can get caught up or hurt.
5. There are glue guns specifically for use with high temp and low temp glue sticks. Make sure you use the right kind for your gun.
4. Do not use hot glue guns anywhere near flammable material.
3. If there is a crack in the body, frayed wires or some other defect with your glue gun, please stop using it and go buy a new one. Using a defective glue gun increases the chance you will get hurt.
2. Do not use a glue gun on thin or porous materials without a silicone finger sleeve if you need to push any pieces together. The glue will seep through and burn you.
1. Do no use your glue gun while distracted.
witter: @makerhighschool
web: MakerHS.com
Facebook: Facebook.com/Makerhighschool
Intro Music:
“Winner Winner!”
Kevin MacLeod (incompetech.com)
Licensed under Creative Commons: By Attribution 3.0
https://creativecommons.org/licenses/by/3.0/