OEM/ODM Manufacturer Siway MG PU FOAM for Lahore Factories
Short Description:
Description MG PU FOAM is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength; Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins; Key Features 1. Noise silencing effect 2. Strong bonding strength 3. Water & weatherproof 4. Primerless adhesion to most building materials Basic Application 1.Doors and Windows and...
The company keeps to the operation concept "scientific management, high quality and efficiency primacy, customer supreme for OEM/ODM Manufacturer Siway MG PU FOAM for Lahore Factories, Looking to the future, a long way to go, constantly striving to become the all staff with full enthusiasm, one hundred times the confidence and put our company built a beautiful environment, advanced products, quality first-class modern enterprise and work hard!
Description
MG PU FOAM is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength;
Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins;
Key Features
1. Noise silencing effect
2. Strong bonding strength
3. Water & weatherproof
4. Primerless adhesion to most building materials
Basic Application
1.Doors and Windows and wall body between the gap filling sealing, fixed bond
2.Language lab, studio, etc when decorating, gap to fill
Technical data sheet
Project |
Value |
||
Density, Kg/m³,Not less |
10 |
||
Thermal conductivity,35℃,W/(m·K) no more than |
0.050 |
||
Dimensional stability(23±2)℃,48,h no more than |
5 |
||
Operating temperature |
-10~+35℃ |
||
Optimum operating temperature |
+18~+25℃ |
||
Temperature range(After curing) |
-35~+80℃ |
||
Tensile bond strength kPa Not less |
Aluminum plate |
Standard condition,7d |
80 |
Immersion,7d |
60 |
||
PVC plate |
Standard condition,7d |
80 |
|
Immersion,7d |
60 |
||
Cement Plate |
Standard condition,7d |
60 |
|
Shear strength,kpa,Not less |
80 |
||
Foam expansion ratio,Not less |
Standard value-10 |
Certification
JC 936-2004
Color
White
Package
750ml in Bottle * 12 per box
Shelf life
12 months
Note
If you want the TDS or MSDS or other details, please contact with our sales person.
How to vacuum seal mason jars without a vacuum sealer using the hot water bath method.
(Ron speaks quietly so as not to interrupt the other mechanics hard at work in this auto shop.) Hi! I’m Ron Krier from Ron’s Auto Glass. I’m replacing a windshield today from a 2005 Chevrolet Pickup. This was done before… About a year ago. And on this particular model, it was primed but they did not get all the rust spots, they did not get all the rust spots the knife got. What happens is that the metal rots out. Right away! This glass installation is only a year old, and you can see the rust coming in here, from not being primed all the way up. I put some knife marks in there too, as well, to show you the difference. But I will prime mine, where the previous glass installer didn’t prime theirs. That is the problem with doing auto glass and “cutting corners.” I want to let you know that I don’t “cut any corners.” I prime everything after it has been cut open, and before the glass is re-installed.
(Fade To Black)
(Ron speaks quietly again.) I just showed you before the scratches that were in this roofline of this 2005 Chevrolet Pickup Truck. I have now primed the area, all the way across the roofline because there were scratches from a previous glass installation. Now, I have primed the complete area that was covered with rust and scratches. It is now safe for the windshield to be installed into this vehicle. I use Sika Urethane and Glue. It works well together and I have zero problem recommending this product to any of my customers, when they need something fixed or done properly. Ron Krier from Ron’s Auto Glass. I’m looking out for your view.