Hot-selling attractive SV-311 Polyurethane Sealant for Construction Export to Madras

Hot-selling attractive SV-311 Polyurethane Sealant for Construction Export to Madras
  • Hot-selling attractive SV-311 Polyurethane Sealant for Construction Export to MadrasHot-selling attractive SV-311 Polyurethane Sealant for Construction Export to Madras
  • Hot-selling attractive SV-311 Polyurethane Sealant for Construction Export to MadrasHot-selling attractive SV-311 Polyurethane Sealant for Construction Export to Madras

Short Description:

Description SV-311  is a one component polyurethane high modulus flexible sealant formulated as reliable bonding adhesive and joint sealant for construction industry, particularly where a higher modulus and lower movement capacity are required for joints with low or medium movement, e.g. connection joints between floor/stairs and wall, connection joints between floor and machinery, seam sealing / sealing of pipe ducts / ventilation systems, multipurpose joints in metal and wood construction w...


Product Detail

Attentions

Application

Product Tags

Our development depends on the advanced equipment ,excellent talents and continuously strengthened technology forces for Hot-selling attractive SV-311 Polyurethane Sealant for Construction Export to Madras, If you are interested in our products, please feel free to send us your inquiry. We sincerely hope to establish win-win business relationships with you.


Description

SV-311  is a one component polyurethane high modulus flexible sealant formulated as reliable bonding adhesive and joint sealant for construction industry, particularly where a higher modulus and lower movement capacity are required for joints with low or medium movement, e.g. connection joints between floor/stairs and wall, connection joints between floor and machinery, seam sealing / sealing of pipe ducts / ventilation systems, multipurpose joints in metal and wood construction work.

 

Key Features

1. Non-sag consistency 

2. Excellent adhesion to most common building materials

3. High tear strength 

4. High tensile strength

5. Less fluid migration to porous material

 

Technical data sheet
Test standard Test project Unit value
GB13477 density g/m³ 1.20±0.1
GB13477 Flow, sagging or vertical flow mm 0
GB13477 surface drying time(25℃,50%R.H.) min 30
  Curing speed mm/24h 3
GB13477 Durometer Hardness Shore A 25-35
GB13477 100% tensile strength Mpa ≤0.4
GB13477 The elastic recovery rate % 80
  Maximum seam width mm 35
  Minimum seam width mm 8

Color

White, black, grey

 

Package

300ml plastic cartridges and 600ml in sausage

 

Shelf life

9 months 

 

Note

If you want the TDS or MSDS or other details, please contact with our sales person.

  • Previous:
  • Next:



  • Gorcci is producing and exporting one component polyurethane foam (PU foam), silicone sealant, PU sealant, no more nails, acrylic sealant and various type of glue and so on. Welcome to visit www.gorvia.com for more details. info@gorvia.com



    In this video I will showcase the extent of hard water spotting with a beading and sheeting based wax and sealant and compare them to each other. This is a 7 day update for the Turtle Wax ICE Synthetic Paste Polish (2007), and the Corrosion Technologies RejeX Paint Sealant. The day prior to the test, I came out and washed each side down using Meguiar’s Deep Crystal car wash soap, and I examine the spotting that occurred from the sprinkler system on the test sections overnight.

    I’m addressing the specific claim that sheeting based products are better than tighter beading products because they reduce hard water spotting. As you can see from the video, the level of spotting is nearly identical regardless of the type of product on the paint. This is because even though sheeting based products are less hydrophobic than beading ones, they are hydrophobic enough for water to bead up if they aren’t flooded enough to form a flat sheet of water across the entire section.

    Our two main sources of hard water spotting occur out of the hose, or from sprinkler systems. These sources have a high concentration of mineral deposits (mostly calcium or magnesium). When hit with water out of a sprinkler system, it’s unlikely you’ll have a perfect situation to where the water will flood flat across the paint panel to have a reduction in beading. Using water out of the hose, we can see that we can focus water onto the paint in order to create this sheeting behavior to occur, but we are in total control of this process. This leaves us with rain water spotting, which is totally different because rain water is naturally soft. Rain spotting will occur with beading and sheeting products, however the spotting is most often just a rearrangement of the dirt/dust/pollen/contaminants that are already on the paint, that are encapsulated by individual rain water beads that when dried will result in lighter spotting. Be sure to check the acid rain levels in your area, if you notice heavy spotting specifically after a rain shower this is the common culprit.

    Sheeting based products can make it easier to dry the car after washing it, manually flooding the entire paint can result in less water being required to be dried using a microfiber drying towel. However, the assumption that sheeting products are better than beading ones because they will prevent hard water spotting is not a real world conclusion that my test demonstrates. I would also question the extent of increased damage by tighter beading products as having a magnifying glass effect on paint underneath when beading occurs.

    Overall, water spotting is not something that you can entirely avoid by specifically altering the surface tension of the product. As you reduce the surface tension, you get closer to the behavior exhibited by paint that is unprotected. The most important aspect with beading and sheeting products, is how well the paint is protected underneath even though spotting occurs on the top layer of the wax or sealant. And in my test, both products perform very well in how just a simple washing with soap removes all traces of hard water spotting.

    What product is better for your paint? It’s up to you to define your own preferences! I use a large assortment of many beading and sheeting products and most of them work great for me.

    I plan to follow up this test using different products, stay tuned for those results!

    Click this link for part 2 where I test the spotting from ICE Shine Lock Sealant and ICE Paste Wax: https://youtu.be/PF3joA36K6Q

    Check out my other videos as well for more water tests and product reviews!

    Turtle Wax ICE Paste Polish (2007) & Corrosion Technologies RejeX Paint Sealant: https://youtu.be/X2tr38-y5aE?list=UURjVlo1D9eSs9QWXlIPL5eg
    Turtle Wax ICE Paste Wax (2015) & Super Hard Shell Paste Wax: https://youtu.be/ZKZpGkPZl4s
    Turtle Wax ICE Shine Lock Sealant: https://youtu.be/2-KPi804MjM
    Meguiar’s Paint Protect: https://youtu.be/a3bi0EASbiE
    Meguiar’s Ultimate Quik Wax & Ultimate Quik Detailer: https://youtu.be/659ZWjGI2II
    Turtle Wax ICE Liquid Wax & Meguiar’s NXT Tech Wax 2.0: https://youtu.be/XQcCtmAbNOU
    Meguiar’s Ultimate Paste Wax & Turtle Wax ICE Paste Wax: https://youtu.be/m_t2KXIhgzs

    Related Products

    WhatsApp Online Chat !