Hot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech Republic

Hot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech Republic
  • Hot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech RepublicHot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech Republic
  • Hot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech RepublicHot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech Republic
  • Hot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech RepublicHot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech Republic

Short Description:

Description SV-8800 is two components, high modulus; neutral curing silicone sealant specifically developed for assembly of high performance insulated glass units as secondary sealing material.   Where to use It is a two-component silicone that offers variable work life with high bonding strength to maintain the integrity of insulating glass unit, suits both commercial and residential IGU.   Key Features 1. High Modulus 2. UV resistance 3. Low vapor and gas transmission 4. Primerless adhesion...


Product Detail

Attentions

Application

Product Tags

We consistently carry out our spirit of ''Innovation bringing development, Highly-quality ensuring subsistence, Management promoting benefit, Credit attracting customers for Hot sale good quality SV-8800 Silicone Sealant for Insulating Glass Wholesale to Czech Republic, we are looking forward to even greater cooperation with overseas customers based on mutual benefits. Please feel free to contact us for more detail


Description

SV-8800 is two components, high modulus; neutral curing silicone sealant specifically developed for assembly of high performance insulated glass units as secondary sealing material.

 

Where to use

It is a two-component silicone that offers variable work life with high bonding strength to maintain the integrity of insulating glass unit, suits both commercial and residential IGU.

 

Key Features

1. High Modulus

2. UV resistance

3. Low vapor and gas transmission

4. Primerless adhesion to coated glass

5. 100% compatible to SV-8890

 

Technical data sheet

Test standard Test project Unit value
Before curing——25℃,50%R.H.
GB13477 Specific gravity(After mixing)   1.33
GB13477 Operating time min 20-40
GB13477 surface drying time(25℃,50%R.H.) min 80-188
corrosivity     No
7 days after curing——25℃,50%R.H.
GB/T 531 Durometer Hardness Shore A 40
GB13477 The tensile modulus at 12.5% elongation Mpa 0.18
  The ultimate tensile strength Mpa 0.92
GB13477 Elongation limit (fracture) % 150

 

Certification

GB-24266-2009;

 

Color

Component A(Base) – White, Component B(Catalyst)- Black

 

Package

1. Component A(Base): (190L), Component B(Catalyst) (18.5L)

2. Component A(Base):24.5kg (18L), Component B(Catalyst): 1.9kg (1.8L)

 

Shelf life

12 months

 

Note

If you want the TDS or MSDS or other details, please contact with our sales person.

  • Previous:
  • Next:



  • This video segment will show you how to do a simple fiberglass repair. This demonstration is applicable to any fiberglass product. TAP has a huge selection of fabrics and resins for fiberglassing. To order fiberglass fabrics, go to https://www.tapplastics.com/product/fiberglass/fiberglass_fabrics
    To order acetone, go to https://www.tapplastics.com/product/fiberglass/epoxy_resins/tap_acetone/11
    To order TAP Gel Coat, go to https://www.tapplastics.com/product/fiberglass/gel_coat
    To order Polyester Resins go to https://www.tapplastics.com/product/fiberglass/polyester_resins



    https://www.homebuildingandrepairs.com/fences/index.html click on this link for more information about wood fence construction and home repairs. Watch this video to learn reasons why wood fence posts rot and fall apart. Moisture and water seems to be wood’s worst enemy and let’s face it in nature it’s part of the decomposition process, so there isn’t much we can do about it. However, if you understand what causes the wood post to rot, I’m pretty sure you can figure out a few ways to reduce these problems and extend the life of your fence. In other words, extend the life of your wood fence posts and save money in the future by reducing your future home repair bills. If this sounds good and you’re looking for some more interesting tips and ideas, visit our websites today area

    Related Products

    WhatsApp Online Chat !