Description This product is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength; Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins; Key Features 1. Noise silencing effect 2. Strong bonding strength 3. Water & weatherproof 4. Primerless adhesion to most building materials Basic Application 1.Doors and Windows a...
We not only will try our best to offer excellent services to every customer, but also are ready to receive any suggestion offered by our customers for Factory Outlets Siway PU FOAM to Portugal Importers, As we are moving forward, we keep an eye on our ever-expanding product range and make improvement to our services.
Description
This product is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength;
Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins;
Key Features
1. Noise silencing effect
2. Strong bonding strength
3. Water & weatherproof
4. Primerless adhesion to most building materials
Basic Application
1.Doors and Windows and wall body between the gap filling sealing, fixed bond
2.Language lab, studio, etc when decorating, gap to fill
Technical data sheet
Project |
Value |
||
Density, Kg/m³,Not less |
10 |
||
Thermal conductivity,35℃,W/(m·K) no more than |
0.050 |
||
Dimensional stability(23±2)℃,48,h no more than |
5 |
||
Operating temperature |
-10~+35℃ |
||
Optimum operating temperature |
+18~+25℃ |
||
Temperature range(After curing) |
-35~+80℃ |
||
Tensile bond strength kPa Not less |
Aluminum plate |
Standard condition,7d |
80 |
Immersion,7d |
60 |
||
PVC plate |
Standard condition,7d |
80 |
|
Immersion,7d |
60 |
||
Cement Plate |
Standard condition,7d |
60 |
|
Shear strength,kpa,Not less |
80 |
||
Foam expansion ratio,Not less |
Standard value-10 |
Certification
JC 936-2004
Color
White
Package
750ml in Bottle * 12 per box
Shelf life
12 months
Note
If you want the TDS or MSDS or other details, please contact with our sales person.
Crash Course on bottom dam issues and fiberglass surrounds. Fastglass is located in southern California. Dana Point CaliforniaFRAMELESS SHOWER ENCLOSURES WITH THIS TYPE OF FIBERGLASS BOTTOM DAM DO QUITE POORLY HOLDING WATER IN CHECK. THE PROBLEM IS THE DESIGN OF THE DAM.THE DESIGN IS PERFECT FOR A FRAMED SHOWER UNIT NOT A FRAMELESS SHOWER. AS YOU CAN IMAGINE WHEN A GOOD TILE OR STONE SLAB IS USED FOR A BOTTOM SHOWER DAM IT HAS THE CORRECT TILT FORCING WATER BACK TO THE DRAIN.TO SOLVE THE LEAK PROBLEM I HAVE BEEN USING ALUMINUM EXTRUSIONS LIKE THE ONE YOU SEE HERE. HOWEVER, I SOMETIMES GET BUSY AND MY AWESOME SHOWER DOOR CREW WILL MEASURE AND INSTALL A SHOWER WITHOUT MY HELP.
Electronic potting compound silicone rubber are the two-component electronic encapsulants with low viscosity with flame Resistance and thermal conductivity.It can be cured under room temperature or heated.Higher the temperature,faster the curing speed.The raw material with higher purity, does not contain any polar compounds and does not produce any By-products, so it can remain the better electrical performance in the hard conditions. It can be applied to pthe surface of olycarbonate, PP, ABS, PVC and metal material, and also for Insulation, moisture-proof, waterproof, shockproof, electronic components, Typical uses for protection of module power supply and circuit board potting high-power electronic components which has high requirements for elimination of heat and high temperature resistance.
The price is USD6.98-11.25/kg. If any interest in it, pls feel free to contact Kitty.
Tel:86-755-89948294
Mob:86-18938867593
E-mail: hyjz(at)szrl(dot)net
Skype:kity-467707861