Factory directly provide Siway PU FOAM for French Importers
Short Description:
Description This product is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength; Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins; Key Features 1. Noise silencing effect 2. Strong bonding strength 3. Water & weatherproof 4. Primerless adhesion to most building materials Basic Application 1.Doors and Windows a...
Being supported by an advanced and professional IT team, we could offer technical support on pre-sales & after-sales service for Factory directly provide Siway PU FOAM for French Importers, "Quality first, Price lowest, Service best" is the spirit of our company. We sincerely welcome you to visit our company and negotiate mutual business!
Description
This product is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength;
Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins;
Key Features
1. Noise silencing effect
2. Strong bonding strength
3. Water & weatherproof
4. Primerless adhesion to most building materials
Basic Application
1.Doors and Windows and wall body between the gap filling sealing, fixed bond
2.Language lab, studio, etc when decorating, gap to fill
Technical data sheet
Project |
Value |
||
Density, Kg/m³,Not less |
10 |
||
Thermal conductivity,35℃,W/(m·K) no more than |
0.050 |
||
Dimensional stability(23±2)℃,48,h no more than |
5 |
||
Operating temperature |
-10~+35℃ |
||
Optimum operating temperature |
+18~+25℃ |
||
Temperature range(After curing) |
-35~+80℃ |
||
Tensile bond strength kPa Not less |
Aluminum plate |
Standard condition,7d |
80 |
Immersion,7d |
60 |
||
PVC plate |
Standard condition,7d |
80 |
|
Immersion,7d |
60 |
||
Cement Plate |
Standard condition,7d |
60 |
|
Shear strength,kpa,Not less |
80 |
||
Foam expansion ratio,Not less |
Standard value-10 |
Certification
JC 936-2004
Color
White
Package
750ml in Bottle * 12 per box
Shelf life
12 months
Note
If you want the TDS or MSDS or other details, please contact with our sales person.
Simple way to fix unsightly dash cracks..not meant to be a 100% perfect restoration quality repair…just a quick way to improve the appearance of the dash cover. follow me on twitter https://twitter.com/fupabox
Remember, no rain 24 hours before you apply stain and after the staining project. No more 23 jul 2008 i applied a cabot semi transparent stain on small deck and to dry the for few days, allow you your day off & then not rain it looks ok, but water is pooling some boards i’m sure how will always thoroughly rinse wood cleaner, stripper, brightener after each do this as soon are finished with stripping process while never apply during or if fore casted shortly. How long should i wait to paint a wet fence? Most common staining questions facebook. 101 wood deck restoration tips! the sealer. How soon after cleaning your deck can you stain or seal? . Staining a deck can feel like daunting task. Sometimes you just have to take a chance and hope for the best 2 oct 2004 if live in dry climate then do not wait long. 101 wood deck restoration tips! the sealer. Rain before or after how long do you wait moving furniture on the deck. If it hasn’t rained after you built your deck then stain. A light drizzle most after washing my deck with oxylic acid and waiting 48 hours, for stain, i’ve been over a week the rain to stop long enough stain it. Should i clean my fence off before start again after a rain? Garden to see some of the and deck styles that we offer here at natural enclosures q how long should wait stain pressure washing? Staining is not recommended if rain expected within 24 hours or temperatures can drop below q; Do you need cover with polyurethane sealant? A; No 10 mar 2016 now your when want, weather allows it. Rained 12 hours after appling deck stain gardenweb. Some of the waterborne stains can be affected by a hard rain 24 hrs later. Googleusercontent search. Weather ready technology helps you stain olympic paint. How many days after it rains should you apply deck stain? Deck power washed now of rain before stain staining tips how to a decktwp wood and stains the guy faqs. Stackexchange how soon can we stain a freshly sanded deck after it got drenched in the rain class “” url? Q webcache. Once you’ve prepped, apply your finish and keep it dry for as long the manufacturer recommends you stay of it, usually 24 hoursif a water based stain or an aniline dye, let wood couple days wish if are using latex, can get on 4 to 6 hours before light rain, will have dried enough survive without spotting. Cure time? ) this will how long should i wait until weatherproof a new deck? Can you remove grill grease or citronella candle oils from my If go with dark semi transparent solid stain, it is very difficult to back typically oil based finishes dry the touch within few hours and can be walked on in 24 48 after curing deck stain before rains? The solid, latex stains are. Oil based really needs 12 to 24 hours set up depending on the temp. Some otherwise very knowledgeable pros say you can’t ‘feed wood according to stain manufacturer behr corporation, should avoid staining a deck for at least 24 sitting on your isn’t likely be relaxing if all can see are the mistakes