Best-Selling CV-709 silicone sealant for PV moudels to azerbaijan Factory
Short Description:
Description CV709 is a high-performance silicone sealant, one-component oxime type room temperature curing silicone rubber, has excellent weather resistance, high thixotropy, after curing for solar components involved in the base material has good caking property, by TUV for environmental requirements of the ROHS, UL E339949 Key Features 1. 100% silicone 2. No sag 3. high thixotropy 4. Water & weatherproof 5. For solar components involved in the base material has good bonding Basic Ap...
With our excellent management, strong technical capability and strict quality control system, we continue to provide our clients with reliable quality, reasonable prices and excellent services. We aim at becoming one of your most reliable partners and earning your satisfaction for Best-Selling CV-709 silicone sealant for PV moudels to azerbaijan Factory, We sincerely welcome overseas customers to consult for the long-term cooperation and the mutual development.
Description
CV709 is a high-performance silicone sealant, one-component oxime type room temperature curing silicone rubber, has excellent weather resistance, high thixotropy, after curing for solar components involved in the base material has good caking property, by TUV for environmental requirements of the ROHS, UL E339949
Key Features
1. 100% silicone
2. No sag
3. high thixotropy
4. Water & weatherproof
5. For solar components involved in the base material has good bonding
Basic Application
1.Solar module frame seal
2.The adhesive of the solar energy back to the terminal block
3.General industrial assembly with seal
Technical data sheet
Test standard | Test project | Unit | value |
Before curing——25℃,50%R.H. | |||
specific gravity | g/ml | 1.34-1.40 | |
GB13477 | Operating time | min | 15 |
GB13477 | surface drying time(25℃,50%R.H.) | min | 40-60 |
3 days after curing——25℃,50%R.H. | |||
Temperature range | ℃ | -55~200 | |
GB13477 | Durometer Hardness | Shore A | 40~55 |
The ultimate tensile strength | Mpa | ≥2 | |
GB13477 | Breaking elongation | % | 300-600 |
Aluminum bonding shear strength | Mpa | ≥1.5 | |
Electrical properties | |||
Breakdown voltage | Kv/mm | ≥20 | |
Volume resistance | ohm.cm | 9E+14 | |
Dielectric constant | 3.1@50Hz |
Certification
UL E339949; TUV
Color
Black, White
Package
300ml in cartridge * 24 per box, 500ml in sausage *20 per box
Shelf life
12 months
Note
If you want the TDS or MSDS or other details, please contact with our sales person.
I did not work for me. Maybe I did it to long.
Instructions I found on the web after I did it.
Firstly you need to boil some water and make sure it is boiling hot.
Remove the rubber from the case and put in the boiling water for about 30sec – 1 min.
Remove the rubber from the boiling hot water and put on ice cold water for about 10-20 sec.
Dry the silicone case with paper towel or cloth and then I hope it will be good as new.