2017 Good Quality Siway MG PU FOAM to USA Importers
Short Description:
Description MG PU FOAM is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength; Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins; Key Features 1. Noise silencing effect 2. Strong bonding strength 3. Water & weatherproof 4. Primerless adhesion to most building materials Basic Application 1.Doors and Windows and...
We take "customer-friendly, quality-oriented, integrative, innovative" as objectives. "Truth and honesty" is our management ideal for 2017 Good Quality Siway MG PU FOAM to USA Importers, Our tenet is clear all the time: to deliver high quality product at competitive price to customers around the world. We welcome potential buyers to contact us for OEM and ODM orders
Description
MG PU FOAM is the expansion, moisture curing, has the strong cohesiveness, elastic foam obturator structure; Save work to save time, reduce waste; High bond strength;
Bubble can stick in the concrete, wood, metal, plastic, such as base material surface, but not including teflon, silicon resins;
Key Features
1. Noise silencing effect
2. Strong bonding strength
3. Water & weatherproof
4. Primerless adhesion to most building materials
Basic Application
1.Doors and Windows and wall body between the gap filling sealing, fixed bond
2.Language lab, studio, etc when decorating, gap to fill
Technical data sheet
Project |
Value |
||
Density, Kg/m³,Not less |
10 |
||
Thermal conductivity,35℃,W/(m·K) no more than |
0.050 |
||
Dimensional stability(23±2)℃,48,h no more than |
5 |
||
Operating temperature |
-10~+35℃ |
||
Optimum operating temperature |
+18~+25℃ |
||
Temperature range(After curing) |
-35~+80℃ |
||
Tensile bond strength kPa Not less |
Aluminum plate |
Standard condition,7d |
80 |
Immersion,7d |
60 |
||
PVC plate |
Standard condition,7d |
80 |
|
Immersion,7d |
60 |
||
Cement Plate |
Standard condition,7d |
60 |
|
Shear strength,kpa,Not less |
80 |
||
Foam expansion ratio,Not less |
Standard value-10 |
Certification
JC 936-2004
Color
White
Package
750ml in Bottle * 12 per box
Shelf life
12 months
Note
If you want the TDS or MSDS or other details, please contact with our sales person.
This is a sequel to the “dryer vent: bad idea” video inwhich I set a cheap dryer vent on fire in the driveway. This is the RIGHT way to do it. A couple notes: why clamps not screws? Because screws give something for lint to snag on in the vent! Why avoid hard 90 degree turns? Because each 90 is like adding five feet to the run. Check your dryer owners manual for the maximum horizontal run supported by the dryer fan. Add up the distances and add 5 feet for each 90 and you have your total. If it goes too far, the exhaust loses speed and the lint falls out. It will also lose heat and cause condensation in the vent leading it to rust and fail.
Here is an affiliate link to what I purchased. If you use this link, I may receive a small commission which helps to pay for making more videos. Thank You.
If you’re shopping for proper dryer vent material, here are a few Amazon links to help you out:
Whirlpool 4396033RP 5-Feet Simple Connect Dryer Vent
https://www.amazon.com/dp/product/B002R0DXMI/?&tag=g07de-20
Whirlpool 4396037RP 0-to-18-Inch Vent Periscope
https://www.amazon.com/dp/product/B001AAEG6S/?&tag=g07de-20